MaximaLabs
Simulation gallery

Guemassa-type cobalt refinery (representative): arsenide leach, scorodite, Cu EW, Cyanex 272, Co EW, CoSO4, Ni(OH)2

HydrometallurgyCobaltArsenicScoroditeElectrowinningSolvent extractionNickelCobalt sulphate
See it live
Open this exact flowsheet in the workspace, already solved — tweak a spec and re-run.
Launch interactive model

A representative Bou-Azzer/Guemassa-type cobalt refinery, not Managem's plant. Managem's Bou-Azzer mine supplies most of the cobalt concentrate its Guemassa hydrometallurgical plants turn into cobalt cathodes, cobalt derivatives and nickel (managemgroup.com, read 2026-10-23), and La Vie Eco (30 December 2025, read) reports a cobalt sulphate unit there of up to 5,800 t/y, from Bou-Azzer metal, entering service in 2026. The plant's own flowsheet and operating figures are not public, so every plant number here is labelled representative. The feed is read from a source: the Bou Azzer concentrate Managem supplied for study, 91.9 g/kg Co, 598 As, 84.3 Fe, 17.5 Ni, 1.9 Cu and 8.1 S (Johnson et al., Hydrometallurgy 2020, Table 1), a skutterudite/loellingite arsenide. Its Fe:As molar ratio comes out 0.19, as that paper states, against about 1 needed to fix arsenic as scorodite. 0.80 kg/s of it (about 2,300 t/y of contained cobalt, the district's output in the same paper) is leached in sulfuric acid at 90 C (95% extraction and the even As(III)/As(V) split are representative inputs), giving a liquor of about 25 g/L As. The arsenic_precipitation unit then oxidises the As(III) and Fe(II) with 50% H2O2 (3.6 mol/s, the stoichiometric demand, drawn from the supply with the rest returned), tops the iron up with ferric sulfate to Fe:As 1.1 (5.5 mol/s Fe, more iron than the concentrate itself carries, which is why arsenide feeds are usually roasted to arsenic trioxide first), and doses lime to pH 1.8 at 90 C: 1.40 kg/s of scorodite and 1.92 kg/s of gypsum, 0.02 mg/L As left, on a scorodite solubility product of -26.67 at 90 C (Langmuir, Mahoney & Rowson's -25.83 at 25 C carried by the temperature dependence of Zhu, Nordstrom et al. 2017). The residue's equilibrium arsenic in TCLP fluid #1 (pH 4.93, 20 L/kg) is 0.03 mg/L against the 5 mg/L toxicity characteristic. A second stage takes the excess iron out as ferrihydrite at pH 4 with lime. Copper is plated potentiostatically (-0.05 V, plug flow, 92% removed), the liquor is neutralised to pH 5 with caustic, and Cyanex 272 at pH 5 (Liu et al. 2021 isotherms) takes all the cobalt and 0.4% of the nickel. The strip liquor, made up with fresh acid and 75% of the spent electrolyte (recycled), is split: 66% goes to cobalt sulphate, where water is removed (87.5%, a specified removal) and CoSO4.7H2O crystallises at 30 C to Seidell's solubility (42.26 g CoSO4 per 100 g water), the mother liquor recycled with a 5% bleed: 0.185 kg/s, about 5,826 t/y, at 95.2% purity with 5% mother liquor in the cake. The rest goes to cobalt electrowinning at 90% current efficiency and 3.2 V, which is 3.23 kWh/kg: the US Bureau of Mines measured 1.48 kWh/lb (3.26 kWh/kg) for cobalt from 75 g/L at 65 C, and about 90% current efficiency. 0.022 kg/s of cathode cobalt (about 692 t/y). Nickel is precipitated from the raffinate as Ni(OH)2 at pH 8.5. Copper is won as cathode, not as copper sulphate: at 1.9 g/kg in the concentrate it never approaches CuSO4.5H2O saturation in this liquor. Bounds: the amorphous ferric arsenate constant is a 25 C value; no arsenate adsorption on ferrihydrite; no jarosite; the evaporation is a specified water removal (the brine property package carries dissolved cobalt as an inert solute, so a steam-driven effect would boil this liquor to dryness at one temperature) and its duty is not computed; the CoSO4 solubility is in water, not in the acid mother liquor; the leach, the H2O2 utilisation, the copper cell, the splits and the SX flows are representative; the barren organic is not recycled.

The flowsheet

The solved topology — every unit op's real duty, conversion, or split, read straight off a genuine converged solve.

Concentrate
Leach ACID
solid
acid
PLS
residue
Leach
Leach Residue
H2O2
Ferric Sulfate
LIME 1
liq
ox
Fe
lime
liq
As
xs
AS Scorodite
Scorodite Residue
Unused Reagents 1
LIME 2
liq
ox
Fe
lime
liq
As
xs
FE AS Polish
Ferric Arsenate Residue
Unused LIME 2
electrolyte
spent
cathode
gas
EW CU
Copper Cathode
CU CELL GAS
Caustic
liquor
reagent
out
excess
Neutralizer
Unused Caustic
CO Organic FEED
feed
solv
ext
raff
SX CO
Strip Liquor
feed
solv
ext
raff
Strip
Barren Organic
electrolyte
spent
cathode
gas
EW CO
Cathode Cobalt
Spent Electrolyte
CO CELL GAS
feed
clarified
sludge
NI Precip
Nickel Hydroxide
Barren Liquor
Strip MIX
CO Split
Spent Split
Sulph MIX
EVAP
EVAP Water
feed
solid
liq
CO Cryst
Cobalt Sulphate
ML Split
Mother Liquor Bleed

The stream table

Every stream's flow, temperature, pressure, and composition — real converged numbers, not placeholders.

See it live
Open this exact flowsheet in the workspace, already solved — tweak a spec and re-run.
Launch interactive model

Stop fighting legacy software. Build your first flowsheet in 60 seconds.