Waelz kiln: zinc oxide from electric-arc-furnace dust
A Waelz kiln recovers zinc from electric-arc-furnace dust: coke reduces the zinc oxide and zinc ferrite in the bed, the zinc vapour burns back to zinc oxide in the freeboard and leaves with the gas as Waelz oxide, and the iron, lime and silica leave as clinker. The charge is the EU BREF on Non-Ferrous Metals (2017) Table 6.4 ratio for an SDHL Waelz plant: 2.68 kg/s of dust, 0.48 kg/s of coke breeze and 0.21 kg/s of lime, which the BREF says gives 1 t of Waelz oxide and 1.63 t of slag. The BREF does not give the dust, so it is REPRESENTATIVE: 25% Zn (inside the BREF's 13-30%), 40% of it as ferrite, 3% Pb, the other oxides lumped as MgO. With 90% of the zinc and lead fumed, half the iron metallized, all spare coke burnt (as SDHL does) and 5% of the clinker carried over, the kiln makes 0.92 kg/s of Waelz oxide at 65.6% Zn and 7.9% Pb, inside the 55-70% Zn the BREF gives for Waelz oxide fed to a zinc plant (Table 6.2), and 1.81 kg/s of clinker at 3.5% Zn: 90.5% zinc recovery. The bed reduction absorbs 4.80 MW and the reoxidation and coke burn above it return it; the whole kiln rejects 0.28 MW, close to the zero the BREF implies when it says SDHL needs no natural gas in normal operation. 0.79 kg of coke is fed per kg of zinc fumed, 2.05 times what the reductions consume. Honesty notes: (1) zinc and lead fuming, metallization, burn-out and carry-over are inputs; (2) chlorides, fluorides, alkalis and cadmium, which make unwashed Waelz oxide what it is, are not modelled; (3) the clinker and gas temperatures (1200 °C, 800 °C) are inputs; (4) the dust is representative, so the Table 6.4 products are a consistency check, not a validation.
The flowsheet
The solved topology — every unit op's real duty, conversion, or split, read straight off a genuine converged solve.
The stream table
Every stream's flow, temperature, pressure, and composition — real converged numbers, not placeholders.