MaximaLabs

Roaster (fluidized bed) simulation

concentrate (feed) + air -> calcine, off-gas (SO2, As4O6 vapour), dust

Governing equations

The exact equations the solver works for a roaster (fluidized bed) — the same math shown in the app's "Theory" panel, not a black box.

ZnS+32O2→ZnO+SO2,FeS2+114O2→12Fe2O3+2 SO2ZnS + \tfrac{3}{2}O_2 \rightarrow ZnO + SO_2,\quad FeS_2 + \tfrac{11}{4}O_2 \rightarrow \tfrac12 Fe_2O_3 + 2\,SO_2
FeAsS+52O2→12Fe2O3+14As4O6(g)+SO2FeAsS + \tfrac52 O_2 \rightarrow \tfrac12 Fe_2O_3 + \tfrac14 As_4O_6(g) + SO_2
ξm=Xm Fm,n˙O2,req=12∑prodνO n˙\xi_m = X_m\,F_m,\qquad \dot n_{O_2,req} = \tfrac12 \sum_{prod} \nu_{O}\,\dot n
Q=∑outFihi(T)−∑inFihi(Tin),hi=ΔHf,i∘+∫298.15Tcp,i dTQ = \sum_{out} F_i h_i(T) - \sum_{in} F_i h_i(T_{in}),\quad h_i = \Delta H_{f,i}^{\circ} + \int_{298.15}^{T} c_{p,i}\,dT
pSO2eq=K(T)pO21/2,ZnSO4⇌ZnO+SO2+12O2p_{SO_2}^{eq} = \frac{K(T)}{p_{O_2}^{1/2}},\quad ZnSO_4 \rightleftharpoons ZnO + SO_2 + \tfrac12 O_2
ξm\xi_m
extent of mineral m's roast [mol/s]
XmX_m
conversion of mineral m [-]
FmF_m
mineral m fed [mol/s]
n˙O2,req\dot n_{O_2,req}
oxygen the roast needs [mol/s]
νO\nu_{O}
oxygen atoms in a product [-]
n˙\dot n
product formed [mol/s]
QQ
duty to hold the bed temperature (negative: surplus heat) [W]
FiF_i
molar flow [mol/s]
hih_i
molar enthalpy on the formation basis [J/mol]
ΔHf,i∘\Delta H_{f,i}^{\circ}
standard enthalpy of formation [J/mol]
cp,ic_{p,i}
heat capacity [J/(mol K)]
TT
bed temperature [K]
TinT_{in}
inlet temperature [K]
pSO2eqp_{SO_2}^{eq}
SO2 pressure over ZnSO4 at equilibrium [bar]
K(T)K(T)
equilibrium constant of the sulfate decomposition [bar^1.5]
pO2p_{O_2}
oxygen partial pressure of the off-gas [bar]

Parameters

oxidising roast of sulfide and arsenide concentrate (sphalerite, pyrite, pyrrhotite, galena, arsenopyrite, safflorite, skutterudite, cobaltite) to calcine and SO2 / As4O6 gas, element balances exact, energy on formation enthalpies (Robie & Hemingway 1995, NBS 1982). temperature [K] (required, the bed); conversion [-] (required for each reactive mineral fed: a number or {mineral: fraction}); sulfate_fraction [-] (ZnSO4/PbSO4 share of the zinc/lead, a number or {zinc|lead: fraction}, default 0 = dead roast); ferrite_fraction [-] (ZnO to ZnFe2O4, default 0); so3_fraction [-] (default 0); dust_carryover [-] (calcine to the dust outlet, default 0); cobalt_oxide (auto | Co3O4 | CoO; auto follows the Co3O4/CoO equilibrium at the off-gas oxygen); heats_of_formation [J/mol] ({mineral: value}; replaces the DFT estimates skutterudite and cobaltite carry, and is required for cobalt_arsenate/ferric_arsenate); arsenate_fixation [-] (fraction of the released arsenic kept in the calcine as arsenate, default 0); arsenate (cobalt | iron | calcium, default cobalt; calcium needs quicklime in the feed); molar_masses [kg/mol] (backend-filled, inert solids). Reports air demand and excess air, SO2/O2 strength (wet, dry) and O2/SO2, surplus heat, autogenous flag, adiabatic temperature, calcine S and As, arsenic volatilised, ZnSO4 and Co3O4/CoO equilibria

Example flowsheets that use it

Stop fighting legacy software. Build your first flowsheet in 60 seconds.