Waelz kiln: zinc oxide from electric-arc-furnace dust — a PENG-ROBINSON process flowsheet
A Waelz kiln recovers zinc from electric-arc-furnace dust: coke reduces the zinc oxide and zinc ferrite in the bed, the zinc vapour burns back to zinc oxide in the freeboard and leaves with the gas as Waelz oxide, and the iron, lime and silica leave as clinker. The charge is the EU BREF on Non-Ferrous Metals (2017) Table 6.4 ratio for an SDHL Waelz plant: 2.68 kg/s of dust, 0.48 kg/s of coke breeze and 0.21 kg/s of lime, which the BREF says gives 1 t of Waelz oxide and 1.63 t of slag. The BREF does not give the dust, so it is REPRESENTATIVE: 25% Zn (inside the BREF's 13-30%), 40% of it as ferrite, 3% Pb, the other oxides lumped as MgO. With 90% of the zinc and lead fumed, half the iron metallized, all spare coke burnt (as SDHL does) and 5% of the clinker carried over, the kiln makes 0.92 kg/s of Waelz oxide at 65.6% Zn and 7.9% Pb, inside the 55-70% Zn the BREF gives for Waelz oxide fed to a zinc plant (Table 6.2), and 1.81 kg/s of clinker at 3.5% Zn: 90.5% zinc recovery. The bed reduction absorbs 4.80 MW and the reoxidation and coke burn above it return it; the whole kiln rejects 0.28 MW, close to the zero the BREF implies when it says SDHL needs no natural gas in normal operation. 0.79 kg of coke is fed per kg of zinc fumed, 2.05 times what the reductions consume.
Modeling assumptions & limitations
- 1Zinc and lead fuming, metallization, burn-out and carry-over are inputs
- 2Chlorides, fluorides, alkalis and cadmium, which make unwashed Waelz oxide what it is, are not modelled
- 3The clinker and gas temperatures (1200 °C, 800 °C) are inputs
- 4The dust is representative, so the Table 6.4 products are a consistency check, not a validation.
27 views 0 forks
- Rigorous PENG-ROBINSON thermodynamics, solved by the same engine every simulation runs on.
- 1 unit operations modeled: KILN.
- Focus areas: Zinc, Waelz, Recycling, EAF dust, Pyrometallurgy, Kiln.
- Thermodynamics
- PENG-ROBINSON
- Components
- oxygen, nitrogen, co2, carbon_monoxide, water, zincite, franklinite, hematite, litharge, quicklime, silica, periclase, coke_breeze, metallic_iron
- Unit operations
- KILN
Opens in a new tab, loaded straight into the app — no setup.
Read the step-by-step guideReproduce this exact result from Python — the real client.get_example() → run_and_wait() path, not a mockup.
from flowsim.sdk import FlowSimClient
client = FlowSimClient()
example = client.get_example("waelz-zinc-oxide")
sim = client.create_simulation(example["title"], example["flowsheet"])
result = client.run_and_wait(sim["id"])
print(result["status"]) # "converged"
streams = client.streams(sim["id"])Related models
Cobalt arsenide roasting: de-arsenication, white arsenic and acid-plant gas
A cobalt arsenide concentrate is roasted to drive its arsenic off as As₄O₆ vapour before the calcine is leached for cobalt; the arsenic is recovered from the gas as white arsenic and the sulfur goes on to a sulfuric acid plant. The concentrate is REPRESENTATIVE of a Bou-Azzer-type feed, not an assay: 5.0 kg/s dry of 12% skutterudite (CoAs₃), 8% cobaltite (CoAsS), 30% arsenopyrite (FeAsS), 5% pyrite and 45% quartz (5.3% Co, 27% As), with 6% moisture. The fluidized-bed roaster runs at 700 °C with 30% excess air; how far each mineral roasts is an input (95%, pyrite 98%). It balances every element and the energy on Robie & Hemingway (1995) and NBS (1982) formation enthalpies: the roast releases 14.16 MW, the bed rejects 5.35 MW to its cooling coils (autogenous; with no heat removed the products would leave at 1386 K), and the off-gas carries 6.33% SO₂, 4.88% O₂ and 1.79% As₄O₆. The cobalt leaves as Co₃O₄ because the gas's oxygen keeps it stable below 1169 K. 95% of the arsenic is volatilised and the calcine holds 1.88% As; 30% of the calcine is carried to the boiler as dust. The gas is then cooled to 150 °C, where As₄O₆'s vapour pressure over solid arsenic trioxide is 2.93 Pa (Welch & Duschak 1915, USBM Technical Paper 81, measured 100-300 °C): 99.84% of it condenses and a baghouse at 99% collection gives 1.67 kg/s of white arsenic, 98.84% of the arsenic in the gas. The same cooler run at 200 °C would recover 94.3% and at 250 °C 27.5%, which is why arsenic is collected cold. Cooling takes out 5.12 MW, 0.45 MW of it sublimation heat. Wet gas cleaning and drying remove the rest of the arsenic and the water, leaving 6.97% SO₂ for the converter, which oxidises 98% of it (one bed, an input) for the absorber.
Hajar (Guemassa, Morocco), representative: a Zn-Pb-Cu-Ag massive-sulphide concentrator with sequential lead, copper and zinc flotation
A representative model of the Hajar concentrator at Managem's Guemassa site, 35 km south of Marrakesh, at its original design point: 3,000 t/d of run-of-mine ore at 10.5% Zn, 3% Pb, 0.3% Cu and 60 g/t Ag (mining-technology.com, 'CMG Metal Mine - Hajar'). The plant there grinds in rod and ball mills and floats lead-silver, copper and zinc concentrates in sequence; this flowsheet does the same with the differential flotation model, in which every mineral of a bank has its own rate constant. The ore. Hajar is a pyrrhotite-rich massive sulphide (50-75 vol% pyrrhotite with sphalerite, galena, chalcopyrite and pyrite; Admou et al., Minerals 8:435, 2018). Here it is 60 wt% pyrrhotite (Fe₇S₈, the formula Marcoux et al. 2008 measured at Draa Sfar nearby), 17.5% sphalerite carrying 11.4 mol% FeS (Draa Sfar's measured mean, the same paper), 3.5% galena, 0.87% chalcopyrite, 2% pyrite and quartz for the silicate gangue. Mineral densities are webmineral's. The grades are chosen to give the design head assay exactly; the silver is placed 80% in galena and 20% in chalcopyrite (about 1,386 g/t in each), which is an assumption: a real deportment comes from mineralogy. Grinding. The mill grinds a 2.5 mm F₈₀ to a 75 micron P₈₀ for 1.43 MW (Bond work index 12, representative). At 400 micron grains, 72% of the galena and 76% of the sphalerite reaching the lead rougher sit in liberated particles. Flotation. Lead rougher and two cleaners (galena floats, sphalerite, pyrrhotite and chalcopyrite depressed), then copper rougher and three cleaners on the lead tailings, then the zinc rougher, scavenger and two cleaners (sphalerite activated). Each cleaner's tailings return to the stage before it and the scavenger concentrate to the zinc rougher, so the model solves seven recycles together. Particles are recovered by flotation at a rate set by their composition and by entrainment with the water: the degree of entrainment by size is Zheng, Johnson and Franzidis's measurement in a 3 m3 cell (0.56 at 7 microns, 0.18 at 25, 0.11 at 88), as reported by Ramlall (J. SAIMM 120, 2020), and the cleaners carry a froth recovery of 0.7. Magnetic cleaning of the zinc concentrate. The plant passes it through magnetic separators to reject pyrrhotite, and so does this model: a wet low-intensity separator on the last zinc cleaner's concentrate. The mineral susceptibilities are Rosenblum and Brownfield's Frantz extraction currents (USGS OFR 99-529, Table 1: pyrrhotite 0.01-0.05 A, iron-bearing sphalerite 0.60-1.00 A, chalcopyrite 0.70-1.30 A; galena, pyrite and quartz above 1.70 A) put through McAndrew's calibration K = 20 sin(15 deg)/I^2 x 1e-6 as MineralMate (Heliyon 2022) restates it, and taken as cgs: pyrrhotite 1.3e-4 m3/kg against 1.1e-7 for the sphalerite. The separator's cut (2e-5 m3/kg) and sharpness are representative. It rejects 97% of the pyrrhotite and 5.3% of the sphalerite, the sphalerite locked in pyrrhotite composites, and lifts the zinc concentrate from 47.3% to 52.5% Zn. The result, against Hajar's published figures (68% Pb at 75% recovery, 28% Cu at 70%, 52% Zn at 94%): the lead concentrate is 67.5% Pb at 75.3% recovery with 1,098 g/t Ag, the copper concentrate 27.9% Cu at 69.4%, and the zinc concentrate 52.5% Zn at 92.3%, with 10.6% Fe of which 5.8 points are the iron inside the sphalerite itself and most of the rest pyrite, which no magnetic separator removes. No published Fe assay for a Hajar concentrate was found to check that against. The tailings carry 0.09% Zn and 0.78% Pb. Each concentrate is thickened and filtered to under 10% moisture by mass, the shipping limit the mine quotes. Bounded, and stated. Every rate constant, maximum recovery and water recovery is representative, fitted here to the published grades and recoveries; none was measured on Hajar ore, and a fitted set is one of many that would match six numbers. The zinc circuit's pyrite activation in particular is a fitted value: with pyrrhotite removed magnetically, something non-magnetic must dilute the concentrate to 52% Zn. A composite particle is treated as one mineral against the average of the rest (binary composites); the unfloatable fraction (R-infinity) is redrawn in each bank rather than tracked through the circuit; and the Frantz-derived susceptibilities are screening values, a ferrimagnetic pyrrhotite at the bottom of the Frantz range being outside McAndrew's calibration.
Guemassa-type cobalt refinery, roast-leach route (representative): roaster, white arsenic, calcine leach, scorodite polish, Cu EW, Cyanex 272, Co EW, CoSO4, Ni(OH)2
The guemassa-cobalt-refinery flowsheet with a de-arsenication roast in front of the leach, which is how arsenide concentrates are usually treated: the direct leach has to buy more iron than the concentrate carries to fix its arsenic as scorodite. Everything from the scorodite stage on is the same nodes as the direct-leach example. The concentrate is REPRESENTATIVE: the roasting example's mineralogy (12% skutterudite, 8% cobaltite, 30% arsenopyrite, 5% pyrite, 45% quartz) with nickel and copper as NiO and CuO at the Bou Azzer concentrate's Ni/Co and Cu/Co (Johnson et al. 2020), 1.40 kg/s dry with 6% moisture, sized to carry the direct-leach example's 73.5 g/s of cobalt. The fluidized-bed roaster at 700 C and 30% excess air (95% of each arsenide roasted, pyrite 98%, inputs) releases 3.90 MW and rejects 1.46 MW to its coils; the off-gas carries 6.32% SO₂. Cooled to 150 C, 0.46 kg/s of white arsenic condenses (98.84% of the arsenic in the gas, on Welch & Duschak's measured As₄O₆ vapour pressure); in all, 93.9% of the arsenic fed leaves as white arsenic, 1.1% stays in the gas, which goes to a product labelled 'to acid plant' (the acid plant is the roasting example's), and 5.0% stays in the calcine and dust, at 1.84% As. Calcine and dust are leached in sulfuric acid at 90 C, mineral by mineral (inputs: 95% of the Co₃O₄, NiO, CuO and unroasted sulfides and arsenides, 10% of the hematite; Co₃O₄ dissolving as Co(II) assumes a reductive leach whose reductant is not tracked), consuming 2.00 mol/s of acid. The liquor carries 978 mg/L As against 25,228 mg/L in the direct leach, and the iron the calcine dissolves puts its Fe:As at 1.82, so the scorodite stage buys no ferric iron (0.0 mol/s against 5.5 mol/s in the direct leach) and needs 0.18 mol/s of H₂O₂ (3.6), 3.60 mol/s of lime (11.18) and makes 0.05 kg/s of scorodite (1.40) and 0.61 kg/s of gypsum (1.92), leaving 0.03 mg/L As; its TCLP screen is 0.03 mg/L. The iron the scorodite does not need drops as ferrihydrite at pH 4 (0.021 kg/s). Downstream as in the direct-leach example: 95% of the copper plated, 0.5% of the nickel co-extracted by Cyanex 272, cobalt electrowon at 3.23 kWh/kg (0.022 kg/s of cathode), and CoSO₄.7H2O at 0.185 kg/s, about 5,826 t/y at 95.2% purity. Bounds: the roast conversions, dust carry-over, collection efficiency and leach fractions are inputs; skutterudite and cobaltite run on DFT heats of formation (see the roasting example); nickel and copper enter as oxides because the roaster has no Ni or Cu minerals, so the arsenic of the nickel arsenides a real Bou Azzer concentrate carries is missing; oxygen in the leach is not tracked; the SO₂ is not converted here.
Solids train (crystallize → filter → dry)
An MSMPR crystallizer feeds a cake filter and dryer — the crystal size and cake moisture propagate on the stream's solids payload (pharma / minerals workflow).
Crystallization with agglomeration (distributed CSD)
An MSMPR crystallizer solved with the rigorous distributed population balance (not just moments): the full crystal-size distribution is computed on a size grid, and an agglomeration (aggregation) kernel combines fine crystals into larger ones — coarsening the mass-weighted mean size (d43) and broadening the distribution (CV rises above the growth-only MSMPR value of ~1.0) while conserving mass exactly. The distribution, its coefficient of variation, and d43 propagate on the solid stream into the filter and dryer — the gPROMS/gCRYSTAL capability the moment model structurally cannot provide.
Crystallization + granulation finishing
A continuous MSMPR crystallizer, cake filter, and dryer feed a granulator that grows the dried crystals into free-flowing granules — the finished-product train after the mother liquor and dryer vapor leave.