MaximaLabs

Zinc Process Flowsheets & Simulations

Explore 2 validated, solved Zinc simulation flowsheets in MaximaLabs — real components: oxygen, nitrogen, co2, carbon_monoxide, water, zincite. Open any one directly in your browser.

Solved via: PENG-ROBINSON.

EAF DUST
COKE
LIME
AIR
feed
air
gas
WOx
clk
KILN
SLAG
Waelz Oxide
OFF GAS
Waelz kiln on EAF dust, EU BREF Table 6.4 charge (representative dust)

Waelz kiln: zinc oxide from electric-arc-furnace dust

A Waelz kiln recovers zinc from electric-arc-furnace dust: coke reduces the zinc oxide and zinc ferrite in the bed, the zinc vapour burns back to zinc oxide in the freeboard and leaves with the gas as Waelz oxide, and the iron, lime and silica leave as clinker. The charge is the EU BREF on Non-Ferrous Metals (2017) Table 6.4 ratio for an SDHL Waelz plant: 2.68 kg/s of dust, 0.48 kg/s of coke breeze and 0.21 kg/s of lime, which the BREF says gives 1 t of Waelz oxide and 1.63 t of slag. The BREF does not give the dust, so it is REPRESENTATIVE: 25% Zn (inside the BREF's 13-30%), 40% of it as ferrite, 3% Pb, the other oxides lumped as MgO. With 90% of the zinc and lead fumed, half the iron metallized, all spare coke burnt (as SDHL does) and 5% of the clinker carried over, the kiln makes 0.92 kg/s of Waelz oxide at 65.6% Zn and 7.9% Pb, inside the 55-70% Zn the BREF gives for Waelz oxide fed to a zinc plant (Table 6.2), and 1.81 kg/s of clinker at 3.5% Zn: 90.5% zinc recovery. The bed reduction absorbs 4.80 MW and the reoxidation and coke burn above it return it; the whole kiln rejects 0.28 MW, close to the zero the BREF implies when it says SDHL needs no natural gas in normal operation. 0.79 kg of coke is fed per kg of zinc fumed, 2.05 times what the reductions consume.

8 unit ops • PENG-ROBINSON

27 0

View & open
ORE
MILL
Water
ore
water
conc
tails
PB RGH
PB WASH
ore
water
conc
tails
PB CL1
ore
water
conc
tails
PB CL2
solid
liquor
over
under
PB THK
solid
liquor
cake
filt
PB FIL
PB CONC
ore
water
conc
tails
CU RGH
CU WASH
ore
water
conc
tails
CU CL1
ore
water
conc
tails
CU CL2
ore
water
conc
tails
CU CL3
solid
liquor
over
under
CU THK
solid
liquor
cake
filt
CU FIL
CU CONC
ore
water
conc
tails
ZN RGH
ZN WASH
ore
water
conc
tails
ZN CL1
ore
water
conc
tails
ZN CL2
ore
water
conc
tails
ZN SCV
solid
liquor
over
under
ZN THK
solid
liquor
cake
filt
ZN FIL
ZN CONC
TAIL
Water MIX
Reclaim
ore
water
mags
non-mags
ZN LIMS
PO Reject
Guemassa, Morocco (representative)

Hajar (Guemassa, Morocco), representative: a Zn-Pb-Cu-Ag massive-sulphide concentrator with sequential lead, copper and zinc flotation

A representative model of the Hajar concentrator at Managem's Guemassa site, 35 km south of Marrakesh, at its original design point: 3,000 t/d of run-of-mine ore at 10.5% Zn, 3% Pb, 0.3% Cu and 60 g/t Ag (mining-technology.com, 'CMG Metal Mine - Hajar'). The plant there grinds in rod and ball mills and floats lead-silver, copper and zinc concentrates in sequence; this flowsheet does the same with the differential flotation model, in which every mineral of a bank has its own rate constant. The ore. Hajar is a pyrrhotite-rich massive sulphide (50-75 vol% pyrrhotite with sphalerite, galena, chalcopyrite and pyrite; Admou et al., Minerals 8:435, 2018). Here it is 60 wt% pyrrhotite (Fe₇S₈, the formula Marcoux et al. 2008 measured at Draa Sfar nearby), 17.5% sphalerite carrying 11.4 mol% FeS (Draa Sfar's measured mean, the same paper), 3.5% galena, 0.87% chalcopyrite, 2% pyrite and quartz for the silicate gangue. Mineral densities are webmineral's. The grades are chosen to give the design head assay exactly; the silver is placed 80% in galena and 20% in chalcopyrite (about 1,386 g/t in each), which is an assumption: a real deportment comes from mineralogy. Grinding. The mill grinds a 2.5 mm F₈₀ to a 75 micron P₈₀ for 1.43 MW (Bond work index 12, representative). At 400 micron grains, 72% of the galena and 76% of the sphalerite reaching the lead rougher sit in liberated particles. Flotation. Lead rougher and two cleaners (galena floats, sphalerite, pyrrhotite and chalcopyrite depressed), then copper rougher and three cleaners on the lead tailings, then the zinc rougher, scavenger and two cleaners (sphalerite activated). Each cleaner's tailings return to the stage before it and the scavenger concentrate to the zinc rougher, so the model solves seven recycles together. Particles are recovered by flotation at a rate set by their composition and by entrainment with the water: the degree of entrainment by size is Zheng, Johnson and Franzidis's measurement in a 3 m3 cell (0.56 at 7 microns, 0.18 at 25, 0.11 at 88), as reported by Ramlall (J. SAIMM 120, 2020), and the cleaners carry a froth recovery of 0.7. Magnetic cleaning of the zinc concentrate. The plant passes it through magnetic separators to reject pyrrhotite, and so does this model: a wet low-intensity separator on the last zinc cleaner's concentrate. The mineral susceptibilities are Rosenblum and Brownfield's Frantz extraction currents (USGS OFR 99-529, Table 1: pyrrhotite 0.01-0.05 A, iron-bearing sphalerite 0.60-1.00 A, chalcopyrite 0.70-1.30 A; galena, pyrite and quartz above 1.70 A) put through McAndrew's calibration K = 20 sin(15 deg)/I^2 x 1e-6 as MineralMate (Heliyon 2022) restates it, and taken as cgs: pyrrhotite 1.3e-4 m3/kg against 1.1e-7 for the sphalerite. The separator's cut (2e-5 m3/kg) and sharpness are representative. It rejects 97% of the pyrrhotite and 5.3% of the sphalerite, the sphalerite locked in pyrrhotite composites, and lifts the zinc concentrate from 47.3% to 52.5% Zn. The result, against Hajar's published figures (68% Pb at 75% recovery, 28% Cu at 70%, 52% Zn at 94%): the lead concentrate is 67.5% Pb at 75.3% recovery with 1,098 g/t Ag, the copper concentrate 27.9% Cu at 69.4%, and the zinc concentrate 52.5% Zn at 92.3%, with 10.6% Fe of which 5.8 points are the iron inside the sphalerite itself and most of the rest pyrite, which no magnetic separator removes. No published Fe assay for a Hajar concentrate was found to check that against. The tailings carry 0.09% Zn and 0.78% Pb. Each concentrate is thickened and filtered to under 10% moisture by mass, the shipping limit the mine quotes. Bounded, and stated. Every rate constant, maximum recovery and water recovery is representative, fitted here to the published grades and recoveries; none was measured on Hajar ore, and a fitted set is one of many that would match six numbers. The zinc circuit's pyrite activation in particular is a fitted value: with pyrrhotite removed magnetically, something non-magnetic must dilute the concentrate to 52% Zn. A composite particle is treated as one mineral against the average of the rest (binary composites); the unfloatable fraction (R-infinity) is redrawn in each bank rather than tracked through the circuit; and the Frantz-derived susceptibilities are screening values, a ferrimagnetic pyrrhotite at the bottom of the Frantz range being outside McAndrew's calibration.

31 unit ops • PENG-ROBINSON

24 0

View & open

Stop fighting legacy software. Build your first flowsheet in 60 seconds.