Scorodite Process Flowsheets & Simulations
Explore 2 validated, solved Scorodite simulation flowsheets in MaximaLabs — real components: water, h2so4, so4, cobalt_concentrate, co, ni. Open any one directly in your browser.
Solved via: BRINE.
Guemassa-type cobalt refinery (representative): arsenide leach, scorodite, Cu EW, Cyanex 272, Co EW, CoSO4, Ni(OH)2
A representative Bou-Azzer/Guemassa-type cobalt refinery, not Managem's plant. Managem's Bou-Azzer mine supplies most of the cobalt concentrate its Guemassa hydrometallurgical plants turn into cobalt cathodes, cobalt derivatives and nickel (managemgroup.com, read 2026-10-23), and La Vie Eco (30 December 2025, read) reports a cobalt sulphate unit there of up to 5,800 t/y, from Bou-Azzer metal, entering service in 2026. The plant's own flowsheet and operating figures are not public, so every plant number here is labelled representative. The feed is read from a source: the Bou Azzer concentrate Managem supplied for study, 91.9 g/kg Co, 598 As, 84.3 Fe, 17.5 Ni, 1.9 Cu and 8.1 S (Johnson et al., Hydrometallurgy 2020, Table 1), a skutterudite/loellingite arsenide. Its Fe:As molar ratio comes out 0.19, as that paper states, against about 1 needed to fix arsenic as scorodite. 0.80 kg/s of it (about 2,300 t/y of contained cobalt, the district's output in the same paper) is leached in sulfuric acid at 90 C (95% extraction and the even As(III)/As(V) split are representative inputs), giving a liquor of about 25 g/L As. The arsenic_precipitation unit then oxidises the As(III) and Fe(II) with 50% H₂O₂ (3.6 mol/s, the stoichiometric demand, drawn from the supply with the rest returned), tops the iron up with ferric sulfate to Fe:As 1.1 (5.5 mol/s Fe, more iron than the concentrate itself carries, which is why arsenide feeds are usually roasted to arsenic trioxide first), and doses lime to pH 1.8 at 90 C: 1.40 kg/s of scorodite and 1.92 kg/s of gypsum, 0.02 mg/L As left, on a scorodite solubility product of -26.67 at 90 C (Langmuir, Mahoney & Rowson's -25.83 at 25 C carried by the temperature dependence of Zhu, Nordstrom et al. 2017). The residue's equilibrium arsenic in TCLP fluid #1 (pH 4.93, 20 L/kg) is 0.03 mg/L against the 5 mg/L toxicity characteristic. A second stage takes the excess iron out as ferrihydrite at pH 4 with lime. Copper is plated potentiostatically (-0.05 V, plug flow, 92% removed), the liquor is neutralised to pH 5 with caustic, and Cyanex 272 at pH 5 (Liu et al. 2021 isotherms) takes all the cobalt and 0.4% of the nickel. The strip liquor, made up with fresh acid and 75% of the spent electrolyte (recycled), is split: 66% goes to cobalt sulphate, where water is removed (87.5%, a specified removal) and CoSO₄.7H2O crystallises at 30 C to Seidell's solubility (42.26 g CoSO₄ per 100 g water), the mother liquor recycled with a 5% bleed: 0.185 kg/s, about 5,826 t/y, at 95.2% purity with 5% mother liquor in the cake. The rest goes to cobalt electrowinning at 90% current efficiency and 3.2 V, which is 3.23 kWh/kg: the US Bureau of Mines measured 1.48 kWh/lb (3.26 kWh/kg) for cobalt from 75 g/L at 65 C, and about 90% current efficiency. 0.022 kg/s of cathode cobalt (about 692 t/y). Nickel is precipitated from the raffinate as Ni(OH)2 at pH 8.5. Copper is won as cathode, not as copper sulphate: at 1.9 g/kg in the concentrate it never approaches CuSO₄.5H2O saturation in this liquor. Bounds: the amorphous ferric arsenate constant is a 25 C value; no arsenate adsorption on ferrihydrite; no jarosite; the evaporation is a specified water removal (the brine property package carries dissolved cobalt as an inert solute, so a steam-driven effect would boil this liquor to dryness at one temperature) and its duty is not computed; the CoSO₄ solubility is in water, not in the acid mother liquor; the leach, the H₂O₂ utilisation, the copper cell, the splits and the SX flows are representative; the barren organic is not recycled.
42 unit ops • BRINE
25 0
View & openGuemassa-type cobalt refinery, roast-leach route (representative): roaster, white arsenic, calcine leach, scorodite polish, Cu EW, Cyanex 272, Co EW, CoSO4, Ni(OH)2
The guemassa-cobalt-refinery flowsheet with a de-arsenication roast in front of the leach, which is how arsenide concentrates are usually treated: the direct leach has to buy more iron than the concentrate carries to fix its arsenic as scorodite. Everything from the scorodite stage on is the same nodes as the direct-leach example. The concentrate is REPRESENTATIVE: the roasting example's mineralogy (12% skutterudite, 8% cobaltite, 30% arsenopyrite, 5% pyrite, 45% quartz) with nickel and copper as NiO and CuO at the Bou Azzer concentrate's Ni/Co and Cu/Co (Johnson et al. 2020), 1.40 kg/s dry with 6% moisture, sized to carry the direct-leach example's 73.5 g/s of cobalt. The fluidized-bed roaster at 700 C and 30% excess air (95% of each arsenide roasted, pyrite 98%, inputs) releases 3.90 MW and rejects 1.46 MW to its coils; the off-gas carries 6.32% SO₂. Cooled to 150 C, 0.46 kg/s of white arsenic condenses (98.84% of the arsenic in the gas, on Welch & Duschak's measured As₄O₆ vapour pressure); in all, 93.9% of the arsenic fed leaves as white arsenic, 1.1% stays in the gas, which goes to a product labelled 'to acid plant' (the acid plant is the roasting example's), and 5.0% stays in the calcine and dust, at 1.84% As. Calcine and dust are leached in sulfuric acid at 90 C, mineral by mineral (inputs: 95% of the Co₃O₄, NiO, CuO and unroasted sulfides and arsenides, 10% of the hematite; Co₃O₄ dissolving as Co(II) assumes a reductive leach whose reductant is not tracked), consuming 2.00 mol/s of acid. The liquor carries 978 mg/L As against 25,228 mg/L in the direct leach, and the iron the calcine dissolves puts its Fe:As at 1.82, so the scorodite stage buys no ferric iron (0.0 mol/s against 5.5 mol/s in the direct leach) and needs 0.18 mol/s of H₂O₂ (3.6), 3.60 mol/s of lime (11.18) and makes 0.05 kg/s of scorodite (1.40) and 0.61 kg/s of gypsum (1.92), leaving 0.03 mg/L As; its TCLP screen is 0.03 mg/L. The iron the scorodite does not need drops as ferrihydrite at pH 4 (0.021 kg/s). Downstream as in the direct-leach example: 95% of the copper plated, 0.5% of the nickel co-extracted by Cyanex 272, cobalt electrowon at 3.23 kWh/kg (0.022 kg/s of cathode), and CoSO₄.7H2O at 0.185 kg/s, about 5,826 t/y at 95.2% purity. Bounds: the roast conversions, dust carry-over, collection efficiency and leach fractions are inputs; skutterudite and cobaltite run on DFT heats of formation (see the roasting example); nickel and copper enter as oxides because the roaster has no Ni or Cu minerals, so the arsenic of the nickel arsenides a real Bou Azzer concentrate carries is missing; oxygen in the leach is not tracked; the SO₂ is not converted here.
48 unit ops • BRINE
30 0
View & open